IIT Kharagpur's Centre of Excellence in Advanced Manufacturing Technology (CoEAMT) has developed two groundbreaking AI-enabled non-destructive testing projects for weld defect analysis. These innovations, showcased at the "TechEx 2024" exhibition by Tata Steel, include "iWeld," which accurately identifies weld defects, and "iToFD," revolutionizing defect detection using ultrasonic data. Prof. Surjya K Pal leads the initiative, praising students' dedication. The projects offer promising solutions for industrial challenges, emphasizing CoEAMT's commitment to innovation and collaboration.